From the second batch of the Project MH, spaghetti of 1.5 and 0.5 was produced from ES 26g and 52g.
Production of 1.5 mm did not have any problem while 0.5 production (extrusion) had a problem. Time to time the extrusion was stopped because of some granules stuck inside or above the 0.5 die. So it had to be cleaned each and every time it stops making the process longer.
For Al2O3 project another 4 number of samples (fibers) were prepared and put to the furnace using another program which was changed according to the TGA results.