For the project Arg, another sample of body should be kneaded with fibers inside 6%. Hence, the kneading was started but after some time it was observed that the kneaded was stopped. There was a problem with the power outlet so that the kneading had to be started from the scratch.
Compression test for the third batch of project MH was done. It showed some interesting results. According to that clay with different kinds of silica had different strengths. According to strength,
1. Double layer Silica
2. Single layer Silica
3. Mixed Silica (Double and Single layer)